Gold recovery from anode slime

dc.contributor.advisorTural, Hüseyin
dc.contributor.authorYıldız, Süleyman
dc.date.accessioned2024-08-19T19:41:17Z
dc.date.available2024-08-19T19:41:17Z
dc.date.issued1998
dc.departmentEge Üniversitesi, Fen Bilimleri Enstitüsü, Kimya Ana Bilim Dalıen_US
dc.descriptionBu tezin, veri tabanı üzerinden yayınlanma izni bulunmamaktadır. Yayınlanma izni olmayan tezlerin basılı kopyalarına Üniversite kütüphaneniz aracılığıyla (TÜBESS üzerinden) erişebilirsiniz.en_US
dc.description.abstractin ÖZET ANOT ÇAMURUNDAN ALTIN KAZANIMI YILDIZ, Süleyman Yüksek Lisans Tezi, Kimya Anabilim Dalı Tez Yöneticisi : Prof.Dr.Hüseyin TURAL Eylül- 1998, 25 sayfa Bu çalışmada anot çamuru değişik derişimdeki nitrik asit ile oda sıcaklığında ve kaynatılarak liç edildi. Böylece en uygun liç şartlan elde edilmiştir. Nitrik asitte çözünmeyen kan kısım altın suyu ile reaksiyona sokuldu. Çözeltide bulunan altın önce Fe (NH4)2(S04)2 ile çöktürüldü. Altın çökeleği tekrardan altın suyu ile çözüldü, ikinci olarak oksalik asit ile çöktürüldü. Böylece %99.7 saflıkta altın elde edildi. Nitrik asit liçinden sonraki gümüş içeren çözelti NaCl ile AgCİ çökeleği oluşturmak üzere reaksiyona sokuldu. MTA sonuçlarına göre, çamurda bulunan gümüşün %91'i geri kazanılmıştır. Kaynama noktasında ve 8-9 M KNO3 kullanılarak elde edilen altın miktarının MTA'nın sonuçlarına çok yakın olduğu görülmüştüren_US
dc.description.abstractIV ABSTRACT GOLD RECOVERY FROM AxNODE SLIME YILDIZ, Süleyman MSc. in Chemistry Supervisor : Prof.Dr.Hiiseyin TURAL September- 1998, 25 pages In this work, anode slime was leached with various concentrations of HNO3 at room temperature and reflux temperature. Thus, the optimum leaching conditions were determined. The solid residue which did not dissolve in nitric acid was treated with aqua regia. The gold in solution was first precipitated with Fe (NH4)2(S04)2- The precipitated gold was then redissolved with aqua regia and reduced with oxalic acid. Thus, %99.7 purity gold was recovered. The filtrate which contains Ag from the HNO3 leaching process was treated with NaCl to give AgCl precipitate. According to MTA results, %91 of Ag in slime was recovered. The amounts of recovered Au and Ag which were obtained with 8-9M HNO3 at reflux temperature were found to be very close to the MTA results.en_US
dc.identifier.endpage35en_US
dc.identifier.startpage1en_US
dc.identifier.urihttps://hdl.handle.net/11454/86066
dc.identifier.yoktezid77404en_US
dc.language.isoenen_US
dc.publisherEge Üniversitesien_US
dc.relation.publicationcategoryTezen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectKimyaen_US
dc.subjectChemistryen_US
dc.subjectAltınen_US
dc.subjectGolden_US
dc.subjectAnot çamuruen_US
dc.subjectAnode slimeen_US
dc.titleGold recovery from anode slimeen_US
dc.title.alternativeAnot çamurundan altın kazanımıen_US
dc.typeMaster Thesisen_US