Effect of Carbonitriding on Corrosion Resistance of Steel 30MnB5 in Two Acidic Environments

Küçük Resim Yok

Tarih

2017

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Springer

Erişim Hakkı

info:eu-repo/semantics/closedAccess

Özet

Corrosion resistance of steel 30MnB5 is studied after carbonitriding, after conventional quenching, and without treatment. Corrosion tests are performed for from 24 to 168 h in two acidic environments (in a hydrochloric acid solution with 10% mole fraction and in fertilizer-containing soil). It is shown that the rate of corrosion of the steel in both environments after carbonitriding is lower than after quenching).

Açıklama

Anahtar Kelimeler

steel 30MnB5, corrosion resistance, quenching, soil corrosion